Sintered Diamond Compacts with a Cobalt Binder
1 Department of Chemistry and Institute of Geophysics and Planetary Physics, University of California, Los Angeles 90024
Diamond powder can be successfully cemented with cobalt. At 62 kilobars the sintering occurs over the temperature range from 1570° to 1610°C. The maximum microhardness of the compact (